Performance Index of Liquid Resin:

Type of resin (Gardner)(Sec) Unsaturated Polyester Resin – Ortho base
Appearance Clear Liquid
Gel time 12 – 25 min
Gel time terms Curing condition with 0.5% Co. (1%) and 2% MEKP (50%)
Peak Temperature Max 185 °C
Solid Content 62% – 66 %
Viscosity at 25 C 300 – 500 cP
Acid Value 10 – 30 mgKOH/g
Shelf life 6 Month

 

Mechanical properties:

Tensile Strength 50 – 65 MPa (Test Method ISO 527-2)
Elongation  9% – 11% (Test Method ISO 527-2)
Tensile modulus 300 – 550 MPa (Test Method ISO 527-2)
Flexural Strength 95 – 115 MPa (Test Method ISO 178)
Flexural modulus 1300 – 3450 MPa (Test Method ISO 178)
HDT Max 50 – 60 °C (Test Method ASTM D648)
Hardness 35 – 40 Barcol (Test Method ASTM D2583)
Volumetric Shrink Max 1.5% (Test Method ASTM D2566)

 

Product Application:

Bathtube & Toilets
General purpose
Sheets
Furnitures
Polyester parts and artifacts with high flexibility and low shrinkage
Flotations Products (Tixotrop & Pre-Accelerator)
Hand Lay-up

 

Product Description:

Very good mechanical properties
Low Colore
Low activity
Very good flexibility
Low shrinkage
Good adhesion to glass fibers

 

Shelf Life:
This product must be stored in its orginal sealed steel drum in a cold and dry place away from fire, heat source and direct sunlight in temperatures between 5-30 °C. Under these conditions, the shelf life of this product will be maximum 6 months from delivery time.

 

Packaging
200 Kg net in steel drum

 

Remark:
Solid content, Viscosity and other qualitative parameters, are customizable based on customer requirements.

Technical specifications of polyester
Acid Value Resin

10 – 30 mgKOH/g

Appearance Resin

Clear Liquid

Gel time

12 – 25 min

Gel time terms

Curing condition with 0.5% Co (1%) and 2% MEKP (50%)

Peak Temperature

Max 185 °C

Shelf life

6 Month

Solid Content Polyester

62 – 66 %

Type of resin (Gardner)(Sec)

Unsaturated Polyester Resin – Ortho base

Viscosity at 25 C

300 – 500 cP

Mechanical properties
Elongation

9% – 11% (Test Method ISO 527-2)

Flexural modulus

1300 – 3450 MPa (Test Method ISO 178)

Flexural Strength

95 – 115 MPa (Test Method ISO 178)

Hardness

35 – 40 Barcol (Test Method ASTM D2583)

HDT

Max 50 – 60 °C (Test Method ASTM D648)

Tensile modulus

300 – 550 MPa (Test Method ISO 527-2)

Tensile Strength

50 – 65 MPa (Test Method ISO 527-2)

Volumetric Shrink

Max 1.5% (Test Method ASTM D2566)