Performance Index of Liquid Resin:

Type of resin (Gardner)(Sec) Unsaturated Polyester Resin – Ortho Base
Appearance Clear Liquid
Gel time 10 – 18 min
Gel time terms Curing condition with 0.5% Co. (1%) and 2% MEKP (50%)
Peak Temperature Max 170 °C
Solid Content 62% – 66%
Viscosity at 25 C 400 – 500 cP
Acid Value 20 – 30 mgKOH/g
Shelf life 6 Month

 

Mechanical properties:

Tensile Strength 45 – 55 MPa (Test Method ISO 527-2)
Elongation  8/50% (Test Method ISO 527-2)
Tensile modulus 420 MPa (Test Method ISO 527-2)
Flexural Strength 80 – 90 MPa (Test Method ISO 178)
Flexural modulus 1400 MPa (Test Method ISO 178)
HDT 55 – 65 °C (Test Method ASTM D648)
Hardness 35 – 45 Barcol (Test Method ASTM D2583)
Volumetric Shrink Max 1% (Test Method ASTM D2566)

 

Product Application:

Varnishes & Electrical Isulations
High flexible composite parts and equipments

 

Product Description:

Low Colore
Good flexibility
Good Glossy
Good mechanical properties

 

Shelf Life:
This product must be stored in its orginal sealed steel drum in a cold and dry place away from fire, heat source and direct sunlight in temperatures between 5-30 °C. Under these conditions, the shelf life of this product will be maximum 6 months from delivery time.

 

Packaging
200 Kg net in steel drum

 

Remark:
Solid content, Viscosity and other qualitative parameters, are customizable based on customer requirements.

Технические характеристики полиэстера
Acid Value Resin

20 – 30 mgKOH/g

Внешний вид Смола

Чистая жидкость

Время гелеобразования

12 – 18 min

Сроки нанесения геля

Curing condition with 0.5% Co. (1%) and 2% MEKP (50%)

Пиковая температура

Max 170 °C

Срок годности

6 месяцев

Полиэстер с твердым содержанием

62 – 66 %

Тип смолы (Гарднер)(сек)

Unsaturated Polyester Resin – Ortho base

Вязкость при 25 С

400 – 500 cP

Механические свойства
Elongation

8/50% (Test Method ISO 527-2)

Модуль упругости при изгибе

1400 MPa (Test Method ISO 178)

Предел прочности при изгибе

80 – 90 MPa (Test Method ISO 178)

Твердость

35 – 45 Barcol (Test aMethod ASTM D2583)

HDT

55–65°С (Метод испытаний ASTM D648)

Модуль упругости

420 MPa (Test Method ISO 527-2)

Предел прочности

45 – 55 MPa

Volumetric Shrink

Max 1% (Test Method ASTM D2566)

Будьте первым, кто оставит отзыв “Лаки и электроизоляторы”

Ваш адрес email не будет опубликован. Обязательные поля помечены *

Пока нет отзывов.

ЕСТЬ ЛИ У ВАС ВОПРОСЫ?

ЗАДАЙТЕ НАМ СВОЙ ВОПРОС ПО ЭТОЙ ФОРМЕ